性能項(xiàng)目 | 測(cè)試條件 | 測(cè)試方法 | 數(shù)值/描述 | 單位 |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | | ASTM D638/ISO 527 | 130 | kg/cm2(MPa)[Lb/in2] |
拉伸模量 | | ASTM D638/ISO 527 | 6800 | kg/cm2(MPa)[Lb/in2] |
拉伸屈服伸長(zhǎng)率(延伸率) | | ASTM D638/ISO 527 | | % |
拉伸斷裂伸長(zhǎng)率(延伸率) | | ASTM D638/ISO 527 | | % |
彎曲模量(彎曲彈性率) | | ASTM D790/ISO 178 | 6800 | kg/cm2(MPa)[Lb/in2] |
彎曲強(qiáng)度 | | ASTM D790/ISO 178 | 130 | kg/cm2(MPa)[Lb/in2] |
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/4" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/8" 23℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/8" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | 50 | kg·cm/cm(J/M)ft·lb/in |
-30℃(缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
23℃(無缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
-30℃(無缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
物性性能 | 比重(密度) | | ASTM D792/ISO 1183 | 1.5 | |
吸水率 23℃/24H | | ASTM D570/ISO 62 | 0.02 | % |
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | 190 | ℃(℉) |
未退火 | ASTM D648/ISO 75 | | ℃(℉) |
熔點(diǎn) | | - | 275 | ℃(℉) |
燃燒性(率) | | UL94 | | |
線性膨脹系數(shù) | | ASTM D696/ISO 11359 | | mm/mm.℃ |
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | | |
1MHZ | ASTM D150/IEC 60250 | | |
介電損耗 | 100HZ | ASTM D150/IEC 60250 | | |
1MHZ | ASTM D150/IEC 60250 | | |
體積電阻率 | | ASTM D257/IEC 60093 | | Ω.cm |
表面電阻率 | | ASTM D257/IEC 60093 | | Ω |
耐電弧性 | | ASTM D495/IEC 60112 | | |
加工條件 | 干燥條件 | | | 130-150 | 6-8h |
加工溫度 | 射嘴 | | | ℃ |
料筒前段 | | | ℃ |
料筒中段 | | | ℃ |
料筒后段 | | | ℃ |
熔體溫度 | | | 280 | ℃ |
模具溫度 | | | 120-150 | ℃ |
壓力 | 注塑壓力 | | 59 | Mpa |
保壓壓力 | | 68 | Mpa |
背壓 | | 68 | Mpa |
螺桿轉(zhuǎn)速 | | | | rpm |
其他 | 備注 | |
顏色 | |
特性 | 滑動(dòng)性 |
用途 |
本公司供應(yīng)LCP-A430,品牌日本寶理 ,型號(hào) A430。參數(shù)為:牌號(hào)*VFBM01,產(chǎn)地/廠家*日本寶理 ,用途級(jí)別*耐磨級(jí)。質(zhì)量保證,歡迎咨詢洽談。